Apologies. A quick test with a small magnet suggests that the
block is probably aluminium. However there must be something
pre-column that's causing these rust particles. Whatever it is
may be the root of your problem also. You could try tracing the
problem back by inserting pre-filters at various places in the
system, such as at the autosampler and pump outlets. The peek
frit-type filters have minimal dead volumes and so shouldn't
affect system performance too much;-)!